Fiberglass reinforced concrete mix
[DOC File]CFA Guide/Manual - Fibertech
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_474485.html
Back-up Mix: Washed and dried silica sand or other sand having a history of successful use in glass-fiber-reinforced precast concrete panel construction; passing through a No. 20 sieve. Facing Mix: Fine and course aggregate for face mix shall conform to ASTM C 33 except for gradation.
[DOC File]SECTION 3455 - GLASS FIBER REINFORCED CONCRETE
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_06beec.html
3.3 Fiberglass Reinforcement: Alkali-resistant (AR) fiberglass filaments shall be continuously introduced by a premix process into the GFRC mix for all backing coats in a manner to produce a continuously dispersed fiberglass mat reinforcement. Insertion of fiberglass mats or scrims shall not be acceptable.
[DOCX File]ARCAT, Inc.
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_385463.html
Concrete Mix Design: Submitted to Architect/Engineer by the Contractor for review and approval. Calcium chloride will not be allowed in the mix design. ... Material: Fiberglass reinforced polyester resin, using grades of resin and fiberglass considered acceptable for use with septic tank construction.
[DOC File]Commercial Cement Plaster 4 - DS822
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_aec3dc.html
Dryvit CCP Base - Concentrate: A fiberglass reinforced, cement plaster mix utilizing alkali resistant fibers and proprietary cementitious admixtures which is field mixed with clean, graded plaster sand meeting ASTM C 897, water and Dryvit AC-100 activator (when specified).
[DOC File]SECTION 02795 POROUS PAVING
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_0dd401.html
Forms shall allow for tie-in to adjacent concrete via the use of fiberglass reinforced plastic (FRP) reinforcing bar. 3.2 Mixing, hauling and placing. Mix Time: Truck mixers shall be operated at the speed designated as mixing speed by the manufacturer for 75 to 100 revolutions of the drum.
[DOC File]THE FOLLOWING NEW SECTION IS ADDED:
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_967279.html
fiberglass reinforced plastic pile (frpp), ___inch diameter linear foot. fiberglass reinforced plastic lumber (frpl) cubic foot. wrapping is to be paid for under the item fiberglass-concrete composite pile (fccp), ___ inch diameter or fiberglass reinforced plastic pile (frpp), ___inch diameter
[DOCX File]SECTION 03 30 00, CAST-IN-PLACE CONCRETE
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_599b41.html
B.Concrete roads, walks, and similar exterior site work: Section 32 05 23, CEMENT AND CONCRETE FOR EXTERIOR IMPROVEMENTS. 1.3 TESTING AGENCY FOR CONCRETE MIX DESIGN: A.Testing agency for the trial concrete mix design retained and reimbursed by the Contractor and approved by Resident Engineer.
[DOC File]BuildSite
https://info.5y1.org/fiberglass-reinforced-concrete-mix_1_d20485.html
1. Apply One Coat Fiberglass Reinforced Stucco onto the lath working from bottom to top at a minimum thickness of 3/8 inches (10 mm). Force the fiberglass reinforced stucco through the mesh so that it fits the gap between the mesh and wall completely. Screed the stucco surface flat and float, smooth the surface once the stucco has lost its sheen.